Homemade? Vaseline and Naptha (For a thinner, more self leveling consistency).Tincho85 wrote:Test 1... EPIC FAIL
[img]https://c2.staticflickr.com/8/7471/2795 ... 2b91_z.jpg[/img]
After 24hs I attempted to remove the molded part but it stuck so damn well to the mold.
It really needs some sort of release agent that can work with the silicone I'm using (Permatex ultra copper rtv).
Any ideas of a home made or cheap solution? Maybe oil or vaseline?
Cheap? I'd suggest the Smooth-on Universal mold release. it's 13.30$ US online. Of course, that may expand a lot after shipping/duties. But it's a more consistent product, and far easier to apply (Spray on). I also suggest a different high-temp silicone, as the Permatex copper was chosen for a relatively high heat conductivity. Perhaps a tin-cure silicone, such as the Smooth-on Mold-max (Or their Poyo putty), as they are able to stand up to low-temperature metal casting. I don't work for them, but they help us out with material selection and application engineering, for wargaming terrain, just as full disclosure.